BOSITE 5001A User manual

www.heatairwelder.com www.plasticweldingtool.com
Email:chinabosite@yahoo.cn Tel:0086-1516740071 1
BOSITE-5001A Extruding Welder User Manual
(Please read the user ’ s manual before operation, and keep in for reference)
BOSITE-5001A plastic extruding welder is a new kind of heat blast welder introducing the advanced international
technology and being made with extractive technique. Moreover, its technical index has reached the standard of
the foreign products with the same level and filled up the blank in China. Heat blast warm-up and the plastic
welding rod are combined together to enhance the welding strength with their reasonable structure, convenient
operation, continuous welding, high working efficiency and great extruding pressure, therefore they are the ideal
products for welding and processing various thermoplastic plastic.
With different welding shoes, it could be used for
1. Welding and splicing the Plastic can
2. Repairing, splicing and sealing for big plastic pipes and plastic parts.
3. Splicing and repairing for thicker plastic membrane or GEO membrane.
Notice: Danger. Please make sure the pin is plugged out when undone the tools.
It
will result in fire or scald by heating when use the tool wrongly.
1. The voltage in tools should be confirmed with the main voltage in the pin. Supply voltage don ’ t surpassed 10%
more or less in rated tools
2. please install overload electrical equipment or electrical leakage based on the protect principle for users
3. No touching welding nozzle and outer part for fearing scald, and even more don ’ t point heat wind to human
and animal.
4. Keep away the machine from dampness.
5. Please be intent when operating.
Technical data Model:BOSITE-5001A
Voltage: 220V
Power Drive motor: 800/1020W
Heat blast 1600W/3400W
Air volume 500L/min
Temperature wind temperature 20-600 ℃/ Heating temperature while plastic extruding is
300 — 400 ℃
Diameter of welding rod φ 3.0mm /5.0mm

www.heatairwelder.com www.plasticweldingtool.com
Email:chinabosite@yahoo.cn Tel:0086-1516740071 1
Application
Application
Application
Application scope
scope
scope
scope
1. Thermoplastic plastic HDPE.PP. PVDF, especially PE can show the characteristic best.
2.
It
is forbidden to use for electric conduction plastic (PE-EL), which can bring electric conduction short circuit of
machine.
3.
It
can once weld the line with width of more than 10mm and plastic board with 40mm below.
4. This machine is used for the fourth part of the barrel bath and the tub and accords to the standard of the
DVS(Germany Welding Association)
Operation
Operation
Operation
Operation instructions
instructions
instructions
instructions
1. Put the tool to the placement frame, fit with the handle, plug the main pin,
2. Switch the power supply of the hot welder on, set the temperature around 300 ° C when welding, when it is
below 270 ° C, motor would be shut off, above 270 ° C, turn on the motor, it start working. Switch on the hot air
gun, adjust the temperature knob, and then the material in the welding nuzzle will be soften when heat up
about 7 to 8 minutes.
3. Button the switch of the motor and then the motor begin to rotate. Big noise may caused by the resonance
between the machine and seat or the intensity of spare parts inside the machine.
If
the motor move smoothly
and the inside noise disappeared after feeding the material , it is qualified.
4. After motor start up, Keep the machine standby for around 5 to 6 minutes, then feed the welding rod. Adjust the
temperature knob until the plastic rod is totally soften.
5.
It
will rotate easily without plastic rod. While it is heavy after feeding material.
If
it become too heavy, stop the
machine immediately, maybe it is heated not enough.
6. Different welding shoes for different welding method, two standard welding shoes is provided.
7. Press the machine to the welding joint. Extruding few rod to heat the welding shoe, and make the welding joint
surface not smooth.
8. The welding joint performance would be effected by welding speed, material feeding, welding angle and the
design of welding shoe. The strength of the welding joint is depends on the temperature and air volume of
pre-heating. the heat temperature normally is about 260 ’ C-400 ’ C. And, the faster it moves, the higher
temperature it needs.
9.
To
set the suitable temperature is very important, heat the welding material until it loose its original shiny is
enough.
10. Don ’ t knock the chromosorb welding head hardly when replacing it.
It
is better to heat up for a while.
11. Please replace the carbon brush of the heat blast motor in advance since the span is about 800 hours. Pls
change it before it is used up.
12.
It
should adjust the temperature of the heat blast knob to the lowest point when the machine stop using. And it
shouldn ’ t turn the wind motor off until blowing several minutes.
13.
It
keep some welding rod in when stop the machine for fear of the scratch when extruding the screw racing
screw roller.
14.
It
must clean the material in the glue tongue when open the machine.
Maintenance
1.
It
will be fixed for one year since the product BOSITE -5001A Extruding welder is sold out .
2. Users should check the machine whether it is in good shape or not, if it is no news within two days, it will be
viewed as tact and pass the check

www.heatairwelder.com www.plasticweldingtool.com
Email:chinabosite@yahoo.cn Tel:0086-1516740071 1
NO maintenance for the following situation.
31). Users don ’ t timely report to the problem in the operation or don't follow the
Instruction in the manual to take immediately measure to prevent from the bad situation.
2). Users damage or use overload on purpose.
3). Without admit of manufacture, user disassembly the machine and maintenance it by himself .
4). Without the admit of manufacture, user change the structure of add some parts in the structure.
5.) User don ’ t follow the specification in the literary to operate.
6.) Chinaware electric pipe or the production unsold by the company.
4. Normal abrasion or ullage wasn ’ t given to maintenance.
5 . Force majeure (thunder shocking, flooring, fire, accidents and so on) resulting in the damage wasn ’ t promise to
maintenance.
6 .
It
will lost effect itself after the period of maintenance above the items
Maintenance and Service
1) we are promised to maintenance the products sold by our company
2) Our company is responsible for supplying the technical training to customers.
3) The property is owed to the company.
Table of contents
Popular Welding System manuals by other brands

widos
widos 2500 / OD 315 Working Instructions Translation

Vector Welding
Vector Welding C-Series operating instructions

Lincoln Electric
Lincoln Electric VANTAGE IM10044 Operator's manual

Lincoln Electric
Lincoln Electric IM355-C LN-9 GMA Operator's manual

Parkside
Parkside PESG 120 A1 Assembly, operating and safety instructions

ESAB
ESAB A6 Mastertrac instruction manual